I am with Bruce on this - one wants to use the 'hard' surface chrome rings with the iron bores (the bores slowly wear) or use the 'soft' iron rings on the hard Nikasil cylinders (which is a thin, hard coating that can't be overbored, unless the coating is removed and the cylinder is replated.